10 FAQs about One-Component Platinum Curing Agent

Q1: How to determine the proportion of vulcanizing agent added? A: Adjust according to the hardness of the raw material, such as 0.8% for 30°A, 1.8% for above 80°A Q2: What might be the reason for the incomplete vulcanization? A: Contact with nitrogen/phosphorus containing substances, incompatible color glue or too high temperature (>50℃). Q3: Does […]